I've tried several iterations with my equipment and still get pretty bad orange peel.
Spraying Sherwin-Williams Jet Glo polyurethane and their epoxy primer. I'm using HVLP equipment with an Apollo gun and 1.3 mm tip. I have tried varying the settings on the gun, heavier and lighter application, one and two coats with 30 minute flash off per the application sheet. I'm usually spraying at 65 deg farenheit with the appropriate thinners and reducers per direction. Tried the normal amount of thinner / reducer, and increased that to the max recommended for "three coat shoots".
Thanks!
Spraying Sherwin-Williams Jet Glo polyurethane and their epoxy primer. I'm using HVLP equipment with an Apollo gun and 1.3 mm tip. I have tried varying the settings on the gun, heavier and lighter application, one and two coats with 30 minute flash off per the application sheet. I'm usually spraying at 65 deg farenheit with the appropriate thinners and reducers per direction. Tried the normal amount of thinner / reducer, and increased that to the max recommended for "three coat shoots".
Thanks!