Good morning everyone,
I am working on the emp fairing between the HS and VS. It is a good fit, however there are a few areas where the fiberglass doesn't sit flush with the aluminum. I want to fill these to get rid of the warped appearance and was wondering...how much flox (if any) should be added to the resin? I am using the West Systems slow hardener.
thanks in advanced
Brandon
I am working on the emp fairing between the HS and VS. It is a good fit, however there are a few areas where the fiberglass doesn't sit flush with the aluminum. I want to fill these to get rid of the warped appearance and was wondering...how much flox (if any) should be added to the resin? I am using the West Systems slow hardener.
thanks in advanced
Brandon