I'm almost ready to do my first priming session on the HS.
I've decided to go the Alumiprep/Alodine/AKZO epoxy primer route.
A couple of questions:
1) Should I prime the interior skins or leave them naked aluminum? I'm sure the Alclad alone would be fine. Any real benefits here? Formed, bent and extruded parts will definitely get the whole treatment.
2) And if I do prime the interior skins should this be done before dimpling the skins? Will banging away with a C-frame to dimple the skins mess up the primer coating?
3) What is a reasonable amount of primer to prepare to do the HS parts? I don't want to waste this stuff!
Thanks!
I've decided to go the Alumiprep/Alodine/AKZO epoxy primer route.
A couple of questions:
1) Should I prime the interior skins or leave them naked aluminum? I'm sure the Alclad alone would be fine. Any real benefits here? Formed, bent and extruded parts will definitely get the whole treatment.
2) And if I do prime the interior skins should this be done before dimpling the skins? Will banging away with a C-frame to dimple the skins mess up the primer coating?
3) What is a reasonable amount of primer to prepare to do the HS parts? I don't want to waste this stuff!
Thanks!