oren_rokach
Well Known Member
Hello everyone,
i am just about to receive my QB kit, sparyed with SWP60g2 wash primer.
Since i live in a salty humid area (deadly combination ), i wonder if the SW was primer will do the job, or do i need ot consider something else?
1. scuff it all and redo wiht alodyne/epoxy like i did in the empenage? seems problematic sine already rivetted. i will not be able to reach the most important places, where skin touches the ribs...etc
2. spray on top? also seems problematic, since a few months would elapse since coating was done in the Philippians. but maybe better than nothing?
Any recommendation from you prime experts would be greatly appreciate.!
Thanks
Oren.
i am just about to receive my QB kit, sparyed with SWP60g2 wash primer.
Since i live in a salty humid area (deadly combination ), i wonder if the SW was primer will do the job, or do i need ot consider something else?
1. scuff it all and redo wiht alodyne/epoxy like i did in the empenage? seems problematic sine already rivetted. i will not be able to reach the most important places, where skin touches the ribs...etc
2. spray on top? also seems problematic, since a few months would elapse since coating was done in the Philippians. but maybe better than nothing?
Any recommendation from you prime experts would be greatly appreciate.!
Thanks
Oren.