maniago
Well Known Member
As is an option for the M2 kit, I had my wings factory built by a contractor in FL.
I'm now working on hanging the wings and plumbing and found some pitting corrosion on the Alodined main and rear spar - it looks like chicken pox of very small salt mounds. It'll be at least 2yrs before the plane is done and painted, so I need to do something that'll stem the tide but not be an issue for paint. (Its not enough of an issue to go back to the contractor, but enough to want to do something about it).
CorrosionX is pretty liquidy and flows out of the seams - not good in my case. I see BoeshieldT-9 is a waxy substance as is LPS3. Anyone have experience with either of these?
I was thinking of wiping it on with a soaked rag on a long pole for now, then commit to the spray thing once its painted, so whatever product I pick, I need to stick with.
Thoughts?
I'm now working on hanging the wings and plumbing and found some pitting corrosion on the Alodined main and rear spar - it looks like chicken pox of very small salt mounds. It'll be at least 2yrs before the plane is done and painted, so I need to do something that'll stem the tide but not be an issue for paint. (Its not enough of an issue to go back to the contractor, but enough to want to do something about it).
CorrosionX is pretty liquidy and flows out of the seams - not good in my case. I see BoeshieldT-9 is a waxy substance as is LPS3. Anyone have experience with either of these?
I was thinking of wiping it on with a soaked rag on a long pole for now, then commit to the spray thing once its painted, so whatever product I pick, I need to stick with.
Thoughts?