Just posted a couple pictures of my about to be finished -10 HS and I am getting some comments on how I may not be "aggressive" enough. I am using an Experimental Aero dimpler with a dimple die set from Cleveland. Will try to get some pics posted on here...all arrows and suggestions are welcome.
Main question is, is there a difference in the die sets and just how tight can one go when dimpling. Not wanting to cause stress cracks...I am currently deburring and priming before dimpling.
http://cubeupload.com/im/Thunderpig/IMG0172.jpg
http://u.cubeupload.com/Thunderpig/IMG0173.jpg
http://u.cubeupload.com/Thunderpig/IMG0174.jpg
http://u.cubeupload.com/Thunderpig/IMG0175.jpg
http://u.cubeupload.com/Thunderpig/IMG0176.jpg
http://u.cubeupload.com/Thunderpig/IMG0177.jpg
Main question is, is there a difference in the die sets and just how tight can one go when dimpling. Not wanting to cause stress cracks...I am currently deburring and priming before dimpling.
http://cubeupload.com/im/Thunderpig/IMG0172.jpg
http://u.cubeupload.com/Thunderpig/IMG0173.jpg
http://u.cubeupload.com/Thunderpig/IMG0174.jpg
http://u.cubeupload.com/Thunderpig/IMG0175.jpg
http://u.cubeupload.com/Thunderpig/IMG0176.jpg
http://u.cubeupload.com/Thunderpig/IMG0177.jpg
Last edited: