Default Making Metal

I just did my first oil change at 22.5 hours on a rebuilt 0320-H2AD. When I opened the filter for inspection I found some very small metal flakes (less then a millimeter) in the folds of the filter. They are magnetic so not aluminum. I also found some grit (that what I will call it), which I seem to be able to crush so I suspect it is carbon. I am using single weigh mineral oil. Should I be panicking or is it normal to make a small amount of metal during break-in.
__________________
John Collins
South Central PA
RV6A Phase II
Reply With Quote
  #2  
Old 05-07-2006, 06:47 PM
markscogg markscogg is offline
 
Join Date: Mar 2005
Location: Charlotte, NC
Posts: 306
Red face Metal

Don't freak!
More learned people will chime in later on the specifics. But what you describe doesn't sound so bad
Mark
Reply With Quote
  #3  
Old 05-07-2006, 11:04 PM
osxuser's Avatar
osxuser osxuser is offline
 
Join Date: Aug 2005
Location: Pasadena CA
Posts: 2,484
Default

The questions would mainly be HOW MUCH of the tiny metal flakes are there? if it's an insignificant amount (in other words, you can count them, instead of telling me a 1/4 teaspoon) then I wouldn't worry too much. Just change the oil and keep flying it, check that consumption doesn't do anything weird, and change it again in another 25 to see what it looks like then. The black stuff, is carbon, which is completely normal.
__________________
Stephen Samuelian, CFII, A&P IA, CTO
RV4 wing in Jig @ KPOC
RV7 emp built
Reply With Quote
  #4  
Old 05-08-2006, 06:03 AM
collinsj57@adelphia.net collinsj57@adelphia.net is offline
 
Join Date: Jan 2005
Posts: 136
Default Number of bits (Metal)

I can count them, there might be 35 - 50 or so. not every fold has a piece. No where near a 1/4 tea spoon full. They are magnetic but only slightly and I only checked a few ,some might be aluminum. I am thinking this may be metal from the rings. Oil consumption is good. A little over 1q in 22.5 hours. The case was machined when the T mod was installed before rebuild.????
__________________
John Collins
South Central PA
RV6A Phase II
Reply With Quote
Reply



Posting Rules
You may not post new threads
You may not post replies
You may not post attachments
You may not edit your posts

vB code is On
Smilies are On
[IMG] code is On
HTML code is Off
Forum Jump


All times are GMT -6. The time now is 01:32 AM.


The VAFForums come to you courtesy Delta Romeo, LLC. By viewing and participating in them you agree to build your plane using standardized methods and practices and to fly it safely and in accordance with the laws governing the country you are located in.